Determines the amount of carbon residue formed after evaporation and pyrolysis of petroleum materials under certain conditions and is intended to provide some indication of the relative coke forming tendency of such materials.
Conforms to the specifications of: ASTM D4530; ISO 10370; IP 398; DIN 51551
230V 50/60Hz, 1500W
- K41000-2 2 ml borosilicate glass sample vial for micro conradson test
- K41000-3 16 ml borosilicate glass sample for micro conradson test
- K41100-3 16 ml vials (pack of 144) for single use
- K41100-4 2 ml vials (pack of 100) for single use
- Ambient Temperature: 15 to 30°C
- Ambient Relative Humidity: Max 85% (noncondensing)
- Furnace Temperature Range: from ambient temperature to 550°C
- Temperature Measurement Resolution: 1°C
- Furnace Cooling: by compressed air injection
- Maximum load of samples: 12 small vials / 6 large vials
- Power: 1500W, 250x300x600mm (±15kg)
- Maximum Test Temperature: 550°C
- Temperature measurement Resolution: 1°C
- Furnace Cooling: by compressed air injection
- Automatically controlled atmosphere
- Maximum load of samples: 12 small vials / 6 large vials